Welding & Fabrication

Weld Joint Preparation Worksheet

A worksheet for preparing joints: cleaning, beveling, root gaps and material-specific steps.

Why keep this record

Joint preparation determines whether the weld fuses properly. Thick metal needs bevels so that the arc can reach the root. Thin metal needs a clean edge and tight fit. Rust, paint, oil, galvanizing and mill scale contaminate the weld, causing porosity, cracks and poor fusion. A preparation worksheet records what the joint needs, what you did and how you checked it, which is useful when a joint must be repeated or inspected.

Worksheet

JointMetal and thicknessCleaning methodBevel or edge prepRoot gapChecked
Joint A
Joint B
Joint C
Joint D
Joint E
Joint F
Joint G
Joint H
Joint I
Joint J

How to complete it

  1. Identify the joint type on the drawing and the thickness of each part.
  2. Remove coatings, rust and oil with a grinder, wire brush and solvent, going about an inch each side of the weld.
  3. Bevel thick plate to the specified angle, usually about 30 to 37 degrees per side, leaving a small root face.
  4. Set the root gap using spacers or a feeler gauge and tack at the correct spacing.
  5. Check that edges are straight and parts align.
  6. Note any special steps, such as preheating thick or high carbon steel.

A sample entry

Joint C, 3/8 inch plate butt joint. Bevel ground to 30 degrees each side with a 1/16 inch root face. Cleaned to bright metal 1 inch each side. Root gap 3/32 inch with spacers. Tacks every 4 inches, preheat not needed at this thickness in a warm shop.

Reading the results

If welds show lack of fusion at the root, review the bevel and gap. If you see porosity, review cleaning. Link every defect to a step on the worksheet, and adjust the step.

Shop tip

Make a set of sample joints with different gaps and bevels on scrap, weld them and cut or bend them to see inside. These samples teach more than any chart. Keep them labeled on a shelf for training new welders, and for reference when you meet a similar joint.

Common mistakes

  • Cleaning only the surface of the joint and leaving paint or mill scale at the edges.
  • Using a root gap that is too tight and blocks penetration.
  • Beveling at the wrong angle, which makes filler waste and distortion.

Stop and get help if

  • The metal is galvanized or coated with an unknown material.
  • The steel is of unknown composition and may crack.
  • The part is thick and you do not know the preheat needed.

Keeping the record

Galvanized steel must have the zinc ground off before welding, and welding galvanized metal produces hazardous fumes. Use appropriate respiratory protection and ventilation.