Weld Joint Fit-Up Inspection
An inspection sheet for fit-up before welding, covering gaps, alignment, cleanliness and tack welds.
Why keep this record
A good weld starts before the arc. Poor fit-up forces the welder to fill gaps, overheat the joint and chase distortion. Gaps that are too wide cause burn-through and weak welds, and gaps that are too tight prevent penetration. Misaligned edges, dirty surfaces and weak tacks produce defects that no skill can fully fix. Inspect each joint after fit-up and before final welding, and record what you find.
Worksheet
| Joint | Gap | Alignment | Cleanliness | Tack welds | Ready to weld |
|---|---|---|---|---|---|
| Joint 1 | |||||
| Joint 2 | |||||
| Joint 3 | |||||
| Joint 4 | |||||
| Joint 5 | |||||
| Joint 6 | |||||
| Joint 7 | |||||
| Joint 8 | |||||
| Joint 9 | |||||
| Joint 10 |
How to complete it
- Check the drawing for the joint type, gap and angle, then measure each joint with a feeler gauge or a rule.
- Check the alignment of edges and surfaces, and correct high-low offsets that exceed the limit.
- Clean the joint area to bright metal on both sides, removing rust, paint, oil and mill scale.
- Inspect tack welds for size, spacing and cracking, and grind out defective ones.
- Confirm that clamps and fixtures hold the parts in place without forcing distortion.
- Record ready to weld or list the corrections to be made.
A sample entry
Joint 4, fillet of 3/16 plate to a 2 inch tube. Gap 1/16 inch, within limit. Alignment good, mill scale removed. Four tacks, one cracked, ground out and replaced. Clamped at both ends. Ready to weld.
Reading the results
If the same joints fail fit-up, trace the cause back to cutting or layout. Poor fit-up is almost always a symptom of earlier errors. Fixing the source improves welding quality and saves time.
Shop tip
Use a pair of welding magnets or angle clamps to hold the parts square. Check the squareness twice, before and after tacking, since tack welds pull parts. Mark the tack sequence with a paint pen, so you do not forget one, and let tacks cool before the final weld starts.
Common mistakes
- Welding over a cracked tack, which will usually propagate into the final weld.
- Forcing a large gap closed with a clamp and then welding it under stress.
- Skipping cleaning because the metal looks fine.
Stop and get help if
- The gap is far outside the limit for the process.
- Tack welds are cracked.
- The surfaces are contaminated with oil or galvanizing.
Keeping the record
Where gaps are large, build up the edges with weld metal or use a backing strip, instead of trying to fill the gap with a single pass. Avoid forcing parts into place with heat or weld, which locks in stress.