Welding & Fabrication

Cracked Equipment Inspection Log

A log for finding, measuring and tracking cracks in farm equipment before repair.

Why keep this record

A crack is a warning. It means metal has been loaded beyond what it can carry, and it will grow. Cracks in frames, brackets, hitches and implements are often found late, after they have run for inches. A log lets you record where cracks start, how long they are and how fast they grow, which tells you whether a repair is urgent. It also helps you notice patterns across machines, such as repeated cracks at one mount.

Worksheet

EquipmentCrack locationLength and directionDate foundSuspected causeAction
Tractor frame or loader
Implement frame
Hitch or drawbar
Brackets and mounts
Wagon or trailer frame
Feeder or gate
Hydraulic mounts
Axle housings
Shop fixtures
Other

How to complete it

  1. Clean the area around the suspected crack with a wire brush and degreaser so that the edges can be seen.
  2. Mark the ends of the crack with a paint pen and note the date so that growth can be measured.
  3. Use dye penetrant or magnetic methods if available to confirm the crack and see its true length.
  4. Record the location with a photograph, a sketch and a measurement from a fixed point.
  5. Think about the cause: overload, poor weld, fatigue, rust or impact damage.
  6. Decide whether to stop using the equipment, repair it or monitor it, and write the decision.

A sample entry

Loader arm bracket, 3 inch crack at the lower weld toe, found Oct 20 and marked. By Oct 27 the crack had grown 1/2 inch. Suspected cause: overloading in bucket work. Ground out, welded with preheat, added a doubler plate. Rechecked at 20 hours.

Reading the results

A growing crack is an emergency, so stop use until fixed. A stable crack may allow time, but record its length weekly. Repeat cracks in the same location show a design weakness that should be corrected with reinforcement.

Shop tip

Inspect high risk areas after the first hours of every season and after any heavy shock load. A flashlight, a mirror and a magnifier are the main tools. Look for rust stains in a line, paint cracking and bright metal at a joint, which often show before the crack is visible.

Common mistakes

  • Welding over a crack without removing it first.
  • Drilling stop holes and then forgetting to check them.
  • Treating the crack as the problem and not finding what loaded the part.

Stop and get help if

  • The crack is in a structural part that carries people or heavy loads.
  • The crack is growing quickly or has branches.
  • The part is cast iron or heat treated and cannot be welded easily.

Keeping the record

A standard repair is to drill a small hole at each end of a crack to slow growth, then grind a groove and weld. For critical parts, consult an expert. Repairs without finding the cause often fail again.